Material Notes:
Acrylic adhesive with moisture stable PE coated kraft base release and high density PE interliner.Features: Clear releases liner allows easy inspection of back lighted panelsPlasticizer migration resistantChemical resistantApplications: Mounting nameplates, graphic panels and decorative trim. Bonding a wide variety of substrates.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Adhesive
76.2 microns
3.00 mil
Interliner
Mechanical Properties Metric English Comments
Peel Strength 0.614 kN/m
3.50 pli
180° peel, PET/s.s.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 116 °C
240 °F
Shear Adhesive Failure (cohesive failure)
121 °C
250 °F
Continuous
204 °C
400 °F
Intermittent
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Continuous