Lubrizol Advanced Materials PEARLBOND® 104 Linear Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlbond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLBOND® 104 Linear Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Pearlbondâ„¢ 104.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a high thermoplasticity level. It is used for Hot melt adhesives.Application: Pearlbondâ„¢ 104 is mainly used for making heat-sealable fabrics (thermobonding), obtained by coating processes such as scattering or dot-coating (powder or paste). In all cases, the product is previously ground into powder, by cryogenic grinding. The particle size of the powder will depend on the application technique to be used.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Viscosity 2.95e+6 cP

@Temperature 160 °C
2.95e+6 cP

@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Melt Flow 4.0 - 10 g/10 min

@Load 2.16 kg,
Temperature 170 °C
4.0 - 10 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
ISO 868
Thermal Properties Metric English Comments
Melting Point 70.0 - 80.0 °C
158 - 176 °F
MQSA 70 A
Softening Point 65.0 - 70.0 °C
149 - 158 °F
MQSA 70 A
Descriptive Properties Value Comments
Crystallization rate (minutes) High
MQSA 12 B
Thermoplasticity High
MQSA 68 A