ExxonMobil Mobil Rarus 427

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil Rarus 427.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Mobil Rarus 400 Series is a line of premium performance ashless air compressor lubricants designed to meet the stringent requirements of the major compressor manufacturers. They are formulated with high quality mineral base-oils and a high performance additive system designed to provide exceptional equipment protection and reliability for compressors operating under mild to severe conditions. They provide excellent wear protection and the ability to reduce maintenance costs through minimising equipment problems and downstream deposits and carryover. Because of their high FZG Ratings, the Mobil Rarus 400 Series make outstanding lubricants for compressor systems employing gears and bearings making them an excellent selection for crankcases as well as cylinder lubricants. Mobil Rarus 400 Series lubricants exceed the requirements of DIN 51506 VD-L standards and demonstrate a very high resistance to oxidation and deposit formation. They are recommended or approved by many of the leading compressor manufacturers.The Mobil Rarus 400 Series oils are recommended for single and multistage air compressors. They are particularly effective for continuous high temperature operation with discharge temperatures up to 150º C. They are suitable for reciprocating and rotary type machines with the lower viscosity grades mainly used in rotary compressors. Rarus 400 Series oils are recommended for units with a history of excess oil degradation, poor valve performance or deposit formation. They are compatible with all metals used in compressor construction and with mineral-oil compatible elastomers used in seals, O-rings and gaskets. Mobil Rarus 400 Series oils are not intended or recommended for use in air compressors for breathing applications. The following types of compressors have shown excellent performance with the Mobil Rarus 400 Series oils: Reciprocating air compressor crankcases and cylinders; Rotary screw compressors; Rotary vane compressors; Axial and centrifugal compressors; Compressor systems with critical gears and bearings; Compressors used in stationary and mobile applications
Physical Properties Metric English Comments
Density 0.879 g/cc

@Temperature 15.0 °C
0.0318 lb/in³

@Temperature 59.0 °F
ASTM D1298
Viscosity Measurement 100
100
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 104.6 cSt
104.6 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 11.6 cSt
11.6 cSt
ASTM D445
Ash <= 0.010 %
<= 0.010 %
Sulfated Ash, wt%; ASTM D874
Thermal Properties Metric English Comments
Flash Point 264 °C
507 °F
ASTM D92
Descriptive Properties Value Comments
Copper Strip Corrosion 1B
3 hrs @ 100°C
Foam Sequence I, ASTM D989 30/0
FZG 4-Square Load Support, DIN 51354, Fail Stage 11
Rust Prevention, Distilled Water pass
ASTM D665A
Rust Prevention, Synthetic Sea Water pass
ASTM D665B