Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latistat 45/7-02 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer LATI
Trade Name Latistat
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latistat 45/7-02 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dissipative product based on High density polyethylene (HD-PE). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Linear Mold Shrinkage, Flow 0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
Linear Mold Shrinkage, Transverse 0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
Elongation at Break 6.0 %
6.0 %
Elongation at Yield 5.0 %
5.0 %
Tensile Modulus 1.60 GPa
232 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
Charpy Impact, Notched 0.120 J/cm²
0.571 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Vicat Softening Point 90.0 °C

@Load 5.00 kg
194 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 40 ohm
40 ohm
Processing Properties Metric English Comments
Melt Temperature 180 - 230 °C
356 - 446 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa