Kuraray Genestarâ„¢ GP2450NH-2 Nylon, 45% Glass Filled

Category Polymer , Thermoplastic , Nylon
Manufacturer Kuraray Company
Trade Name Genestar™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray Genestarâ„¢ GP2450NH-2 Nylon, 45% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Standard V-0 Grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm.This grade meets UL94, V-0 Flammability rating without Chlorine and Bromine. It has good balance of mechanical properties and flow-ability as well as other V-0 grades containing Bromine Flame Retardant (BFR).
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
Water Absorption 0.80 %
0.80 %
Linear Mold Shrinkage, Flow 0.00040 cm/cm
0.00040 in/in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Spiral Flow 5.50 cm

@Load 750 kg,
Temperature 320 °C
2.17 in

@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
Mechanical Properties Metric English Comments
Tensile Strength 38.0 MPa
5510 psi
Weld; ASTM D638
165 MPa
23900 psi
ASTM D638
Elongation at Yield 0.40 %
0.40 %
Weld; ASTM D638
3.0 %
3.0 %
ASTM D638
Flexural Strength 224 MPa
32500 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 306 °C
583 °F
Deflection Temperature at 1.8 MPa (264 psi) 285 °C
545 °F
ASTM D648
Glass Transition Temp, Tg 125 °C
257 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 30.0 kV/mm
762 kV/in
ASTM D149
Comparative Tracking Index >= 600 V
>= 600 V
ASTM UL746A