| Category | Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate, Molded |
| Manufacturer | Rotuba |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Rotuba MSS Cellulose Acetate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
| Water Absorption | 2.5 % | 2.5 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 31 | 31 | ASTM D785 |
| Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | ASTM D638 |
| Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
| Elongation at Break | 53 % | 53 % | ASTM D638 |
| Flexural Yield Strength | 27.0 MPa | 3920 psi | ASTM D790 |
| Flexural Modulus | 0.0800 GPa | 11.6 ksi | ASTM D790 |
| Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
| 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 138 °C | 280 °F | Flow temperature, ASTM D569 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 180 °C | 356 °F | Center barrel temperature |