M. Holland Company CP502 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company CP502 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Copolymer, High Flow, High Impact ResistanceUses: Closures, Medical Applications, Thin-walled PartsProcessing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.903 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3300 psi
Type I, 2 in/min; ASTM D638
Elongation at Break 8.0 %
8.0 %
Type I, 2 in/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
at 0.05 in/min; ASTM D790
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
at 73°F; ASTM D256
Descriptive Properties Value Comments
Form Pellets