Johnson Matthey JM4060 Soft Solder/Flux

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey JM4060 Soft Solder/Flux.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materials can be offered as solid wires or as flux cored, to suit the required applications. A wide range of Silver containing solders are suitable for applications where higher strength, increased corrosion resistance or electrical conductivity are required. In some markets the use of Lead or Cadmium containing solders is prohibited in potable water systems, this has led to the increase use of the Silver bearing and Copper bearing-Lead free solders. Solders are available as: Sticks wire (solid or flux cored), preforms, ingots, ribbon bars and solder paste. Federal Specification QQ-S-571 40BASTM Grade Sn 40BS.EN 29453 Alloy No. 5Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 183 - 238 °C
361 - 460 °F
Solidus 183 °C
361 °F
Liquidus 238 °C
460 °F
Component Elements Properties Metric English Comments
Lead, Pb 60 %
60 %
Tin, Sn 40 %
40 %