Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials IS802 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, White

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials IS802 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, White.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these paste-consistency products will flow only with external pressure, they may be applied to horizontal, vertical, and overhead surfaces in thicknesses up to 6mm (1/4 in.). They have sufficient uncured body to adhere to small objects while cure is taking place.ISO800 Series adhesives utilize a moisture vapor cure system and release acetic acid vapors from the sealant surface as a by-product of cure.Key Performance Properties: One-component productThixotropic (paste-like) consistencyCapability to cure at room temperature and ambient humidity conditionsExcellent electrical insulation propertiesExcellent weatherability and ozone and chemical resistanceSelf-adhesion propertiesLow temperature flexibilityHigh temperature performanceApplications: The paste-consistency of these adhesive sealants make these products ideally suited for application to vertical and overhead surfaces where use of pourable self-leveling sealants would not be practical. These sealants may be sued in thicknesses up to 6mm (1/4 in.) for bonding and sealing, joining metals and plastics, and electrical insulation.These sealants are not for use in delicate electrical and electronic applications in which corrosion of copper, brass, or other sensitive metals is undesirable.All IS800 series sealants are identical materials, differing only in color.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 23
23
Tensile Strength, Ultimate 2.02 MPa
293 psi
Elongation at Break 450 %
450 %
Adhesive Bond Strength 1.03 MPa
150 psi
Shear, at 100% cohesive failure
Peel Strength 6.49 kN/m
37.0 pli
To anodized aluminum
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+14 ohm-cm
2.50e+14 ohm-cm
Dielectric Constant 2.9

@Frequency 60 Hz
2.9

@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm
508 kV/in
Dissipation Factor 0.0026

@Frequency 60 Hz
0.0026

@Frequency 60 Hz
Processing Properties Metric English Comments
Cure Time 25.0 min
0.417 hour
Tack-free
Descriptive Properties Value Comments
Application rate 410 g/min
Color White
Consistency Soft, spreadable paste