Material Notes:
A high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blowmolding equipment, specifically where applications require excellent environmental stress crack resistance (ESCR). This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D4883
Melt Flow 0.22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 27.6 MPa
4000 psi
2 in/min.; ASTM D638
Elongation at Break >= 700 %
>= 700 %
2 in/min.; ASTM D638
Flexural Modulus 1.034 GPa
150.0 ksi
2% Secant; ASTM D790
1.262 GPa
183.0 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Tensile Impact Strength 233 kJ/m²
111 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D 746
Descriptive Properties Value Comments