Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in per min, tangent; ASTM D638 |
Network Polymers NPP 25-0105 TF20 Description: Copolymer Polypropylene, 20% Talc FilledInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 50-0158 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CR350LN Polypropylene, Random Copolymer COPYLENE™ CR350LN is a high flow random copolymer nucleated and with antistat for good mold release in injection molding applications. Applications: Containers, Closures, HousewaresInformation prov.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CR750CLS Polypropylene Random Copolymer Description: COPYLENE® CR750CLS is a clarified random copolymer specially designed and formulated for clear injection molding applications and is formulated with antistat and lube for excellent mol.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP 301 EXT Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Tensile Strength, Yield | 27.6 - 47.6 MPa | 4000 - 6900 psi | Average value: 35.2 MPa Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Yield | 27.6 - 119 MPa | 4000 - 17300 psi | Average value: 57.1 MPa Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D638 |
Chevron Phillips HiD® 9410 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good TrimabilityApplications:Phar.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2" (50mm) per min.; ASTM D638 Type IV |
Formosa Plastics Formolene® HL5505 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight CopolymerApplications: 55 gallon drums (even those with demanding built-in handling rings), industrial tanksFormolene HL5505 is intended for large part blow molding appli.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D638 |
LyondellBasell Petrothene® LR732013 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D638 |
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D 638 |
LyondellBasell Pro-faxâ„¢ RP320N Polypropylene Copolymer Description: Pro-faxâ„¢ RP320N is a barefoot polypropylene random copolymer designed for cast film packaging applications. Cast film made with this resin has exceptional clarity and gloss, as wel.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D-882 |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1471 Conductive PTFE Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Tensile Strength, Yield | >= 27.6 MPa | >= 4000 psi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.062" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene Impact Copolymer for Extrusion Applications Formolene® 2302E is a low flow, medium impact polypropylene copolymer designed for extrusion applications. It is a barefoot resin with a basic stabilizat.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2" (50mm) per min.; ASTM D638 Type IV |
Formosa Plastics Formolene® HB5502Z Blow Molding HDPE Hexene CopolymerApplications: Injection blow molded pharmaceutical packagingFormolene HB5502Z eliminates the need for including a mold release agent at each machine, by incorporating zinc stearate w.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D-638 |
Axiall Suprel® SVA 9420 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9420 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies .. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D-638 |
Bapolene® 5005H High Density Polyethylene This resin is a high molecular weight, high density copolymer polyethylene resin. Product exhibits superior impact strength and ESCR. Applications: Drums and Industrial Parts.Bapolene® and Bapolan.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in/min (50 mm/min); ASTM D638 |
Bapolene® PP5010 Polypropylene, Extrusion Grade Bapolene PP5010 is an extrusion PP high impact copolymer with excellent color and processability. It offers extra high impact strength and low temperature properties.Applications: Auto, pipe, profi.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D638 |
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded .. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2" per min, Type IV; ASTM D638 |
Amco PRIMATOP HDPE 003955P Phillips Process Hexene Copolymer HDPE 003955P features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco prod.. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | TM R050-36 |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Tensile Strength, Yield | 27.6 MPa | 4000 psi | ASTM D638 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |