Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos ABS Lustran® 723-1, Extrusion Grade  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® 723-1, Extrusion Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Extrusion grade for refrigerator inliner.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Melt Flow 3.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
Elongation at Yield 2.0 %
2.0 %
Tensile Modulus 2.20 GPa
319 ksi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Vicat Softening Point 99.0 °C
210 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Users viewing this material also viewed the following: