| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded |
| Manufacturer | Ineos ABS |
| Trade Name | Lustran® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ineos ABS Lustran® 488.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | |
| Melt Flow | 19 g/10 min @Load 10.0 kg, Temperature 220 °C |
19 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 46.3 MPa | 6720 psi | |
| Elongation at Break | 19 % | 19 % | Nominal |
| Elongation at Yield | 3.5 % | 3.5 % | |
| Tensile Modulus | 2.36 GPa | 342 ksi | |
| Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
|
| Charpy Impact, Notched | 3.20 J/cm² | 15.2 ft-lb/in² | |
| 0.410 J/cm² @Temperature -30.0 °C |
1.95 ft-lb/in² @Temperature -22.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C | 185 °F | |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL Recognized |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
UL Recognized |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 250 °C | 482 °F | Injection Molding |
| Mold Temperature | 60.0 °C | 140 °F | Injection Molding |
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
| Injection Pressure | 55.0 MPa | 7980 psi |