| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 95.0 - 105 °C | 203 - 221 °F | |
|
Fine Organics FINALUX G 785 Lubricant Additive
Applications: External lubricant for rigid PVC calendered, extruded and molded articles with Ca-Zn & Tin stabilizers, synergistic co-stabilizing properties with Ca-Zn stabilizer.Information provided..
|
|||
| Melting Point | 95.0 - 105 °C | 203 - 221 °F | |
|
Fine Organics FINALUX GH 43 Composite Lubricant
Applications: One pack lubricant for Sn & Pb stabilized rigid PVC injection molded articles.Information provided by Fine Organics
|
|||
| Melting Point | 95.0 - 105 °C | 203 - 221 °F | |
|
Fine Organics FINAWAX PE 3 Lubricant Additive
Applications: Oxidised polyethylene wax as an external lubricant for RPVC blown films and extruded products.Information provided by Fine Organics
|
|||
| Melting Point | 95.0 - 115 °C | 203 - 239 °F | |
|
Indium Corp. Indalloy 44 Bismuth Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 95.0 - 136 °C | 203 - 277 °F | |
|
Indium Corp. Indalloy 78 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 95.0 - 137 °C | 203 - 279 °F | |
|
Indium Corp. Indalloy 80 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 95.0 - 104 °C | 203 - 219 °F | |
|
Indium Corp. Indalloy 57 Bismuth Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 95.0 °C | 203 °F | |
|
Techmer ES Plastiblend® ABS 8006
Availability: North AmericaForms: PelletsProcessing Method: Sheet ExtrusionInformation provided by TP Composites, Inc.
|
|||
| Melting Point | 95.0 °C | 203 °F | Freezing Point via DSC/ASTM D3418 |
|
DuPont 20 Series 2010 Specialty Polyethylene Resin
DuPont 2010 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding fl..
|
|||
| Melting Point | 95.0 °C | 203 °F | DSC; ASTM D3418 |
|
DuPont Bynel® 39E660 Adhesive Resin
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
|
|||
| Melting Point | 95.0 °C | 203 °F | Upon Melting via DSC/ASTM D3418 |
|
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown
12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi..
|
|||
| Melting Point | 95.0 °C | 203 °F | ASTM D3417 |
|
DuPont Elvax® 3135XZ Ethylene Vinyl Acetate
DuPont™ Elvax® 3135XZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applicati..
|
|||
| Melting Point | 95.0 °C | 203 °F | ASTM D3417- ISO 3146 |
|
DuPont Elvax® 670 Ethylene Vinyl Acetate
DuPont™ Elvax® 670 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 670 resins can be used for the following applications: molding, compounding ..
|
|||
| Melting Point | 95.0 °C | 203 °F | TRN-14 |
|
Tipco Tipcolite® TPF 1315 - Unreinforced Phenolic Resin having 22 mm Norton Flow with 10% Hexamine
Unreinforced Phenolic Resin having 22mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd.,
Ind..
|
|||
| Melting Point | 95.0 °C | 203 °F | by DSC; ASTM D3418 |
|
Westlake EMAC® Plus SP1307 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1307 is a 20% EMA copolymer designed for extrusion coating, laminations, and blending where EMA properties are needed, but higher temperature resistance is required. SP1307 is..
|
|||
| Melting Point | 95.0 °C | 203 °F | ASTM D3418 |
|
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low..
|
|||
| Melting Point | 95.0 °C | 203 °F | DSC; ASTM D3418 |
|
Westlake Tymax™ GA7001 Anhydride Modified Acrylate Copolymer (Developmental)
Westlake GA7001 is an anhydride modified acrylate copolymer for extrusion coating and cast film tie-layers. This resin is designed to function as a coextruded tie-layer in multilayer applications. W..
|
|||
| Melting Point | 95.0 - 110 °C | 203 - 230 °F | |
|
Goodfellow Roses Metal (Bi, Pb, Sn) Alloy
Fusible alloy. Uses include anchoring, mold applications and fusible links.Information provided by Goodfellow.
|
|||
| Melting Point | 95.0 °C | 203 °F | DSC; ASTM D3418 |
|
DuPont™ Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Surlyn® 1605 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces..
|
|||
| Melting Point | 95.0 °C | 203 °F | Dow Method (DSC) |
|
Dow AFFINITY™ PF 1146G Polyolefin Plastomer (POP)
AFFINITY™ PF 1140G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for high speed packaging applications requiring low seal initiation temperature and good machina..
|
|||
| Melting Point | 95.0 °C | 203 °F | DSC |
|
Arkema Group OREVAC® 9314 EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..
|
|||
| Melting Point | 95.0 °C | 203 °F | DSC; ASTM D3418 |
|
DuPont™ Surlyn® 1705-1 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1705-1 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s..
|
|||
| Melting Point | 95.0 °C | 203 °F | Upon Melting via DSC/ASTM D3418 |
|
DuPont Elvax® 3130SBZ Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **)
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
|
|||
| Melting Point | 95.0 °C | 203 °F | Upon Melting via DSC/ASTM D3418 |
|
DuPont Elvax® 3134Q Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating, Casting
(discontinued **)&l
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
|
|||
| Melting Point | 95.0 - 104 °C | 203 - 219 °F | |
|
Indium Corp. Indalloy 46 Bismuth Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 95.0 °C | 203 °F | Eutectic |
|
Indium Corp. Indalloy 38 Bismuth Solder Alloy
Information Provided by Indium Corporation
|
|||