Indium Corp. Indalloy 189 Aluminum Solder Alloy

Category Metal , Nonferrous Metal , Aluminum Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 189 Aluminum Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 2.75 g/cc
0.0994 lb/in³
Thermal Properties Metric English Comments
Melting Point 521 - 585 °C
970 - 1090 °F
Solidus 521 °C
970 °F
Liquidus 585 °C
1090 °F
Component Elements Properties Metric English Comments
Aluminum, Al 86 %
86 %
Copper, Cu 4.0 %
4.0 %
Silicon, Si 10 %
10 %