Material Notes:
EP1050 is a POSS® based, high-temperature epoxy adhesive with outstanding resistance to ozone, plasma, or atomic oxygen environments. Major applications include medical devices, optics, semiconductors and electronics.Information provided by Hybrid Plastics
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
after cure
Viscosity <= 5000 cP
<= 5000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Modulus of Elasticity 3.00 - 3.50 GPa
435 - 508 ksi
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 100 - 110 °C
212 - 230 °F
Processing Properties Metric English Comments
Cure Time 6.00 min

@Temperature 80.0 °C
0.100 hour

@Temperature 176 °F
Pot Life 180 min
180 min