Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® M48 is a highly toughened epoxy matrix with excellent mechanical and temperature performance, designed specifically for the Motorsport and High Performance Car industry. HexPly® M48 has been developed to have excellent damage tolerance and has evolved from aerospace technology.Features: Highly toughened epoxy matrix, especially at high energy impacts; Elevated temperature performance; Low volatiles; Available on various reinforcements; Excellent drape and tack; Good surface finish; Long shelf life and out-life; Optimum mechanical performance from an autoclave or press cure.
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 15