Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global ABS-0305 General Purpose ABS  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global ABS-0305 General Purpose ABS  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.1 MPa
6100 psi
ASTM D638
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256