Formosa Plastics Formolene® LH6008 Injection Molding HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® LH6008 Injection Molding HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HomopolymerApplications: Totes, cases, crates, over-caps, toysFormolene LH6008 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength, Yield 32.1 MPa
4650 psi
ASTM D882
Flexural Modulus 1.21 GPa
175 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256