Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds GS 7080 Flexible PVC, Injection Molding for Technical Items

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GS 7080 Flexible PVC, Injection Molding for Technical Items.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Plugs
Physical Properties Metric English Comments
Density 1.43 - 1.47 g/cc
0.0517 - 0.0531 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 72
68 - 72
ISO R 868
Tensile Strength at Break 8.00 MPa
1160 psi
ISO R 527
Elongation at Break 200 %
200 %
ISO R 527
Users viewing this material also viewed the following: