3M PS470 White Yupo™ EDP Label Product

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M PS470 White Yupo™ EDP Label Product.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ White Yupo™ EDP Label Products PS470 and PS472 are matte white opaque polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive F2201, which is a freezer grade acrylic that offers high initial tack, good clarity, and adhesion when applied at temperatures as low as 0°F and also has excellent processing characteristics and offers exceptional adhesion to a wide variety of substrates with moderate resistance to water and humidity.Information provided by 3M
Physical Properties Metric English Comments
Thickness 78.7 microns
3.10 mil
Liner
81.3 microns
3.20 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m
2.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
60.0 °C
140 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
-18.0 °C
-0.400 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type F2201 Freezer 16
Liner 50# SC Remoist