Teknor Apex Sinvicomp SRP 5608 Polyvinyl Chloride, Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SRP 5608 Polyvinyl Chloride, Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: Asia Pacific Features: High Gloss; High Impact Resistance Uses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
ASTM D2240
Tensile Strength, Yield 39.2 MPa
5690 psi
9.8 in/min; ASTM D638
Elongation at Break 150 %
150 %
9.8 in/min; ASTM D638
Izod Impact, Notched 1.39 J/cm
2.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C

@Time >=Error in fixSigDigits: @digits must be between 1 a sec
374 °F

@Time >=Error in fixSigDigits: @digits must be between 1 a hour
Congo Red; BS 2782
Vicat Softening Point 93.9 °C
201 °F
ASTM D1525