Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Injection Molding  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Injection Molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be injection molded to produce pliable parts. It can also be used for making alloys, blends, and compounds to increase impact strength or lower modulus.Applications: Injection molding; Compatibilizer and impact modifier for engineering thermoplastics.
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
Exxon Method
Melt Flow 6.0 g/10 min
6.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A >= 90
>= 90
ASTM D2240
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength, Ultimate 12.0 MPa
1740 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Tensile Impact Strength 360 kJ/m²
171 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 102 °C
216 °F
Exxon Method
Vicat Softening Point 78.0 °C
172 °F
1000g; ASTM D-1525