Material Notes:
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior drawdown and enhanced toughness. Enable 20-05 resins are available for blown film, both formulated and non-formulated. A heavily stabilized formulation for cast film processing is also available.Availability: Latin America, North America and South AmericaAdditive::Antiblock: 2000 ppm Slip: 500 ppm Processing Aid: Yes Thermal Stabilizer: YesApplications:Agricultural FilmBlown FilmCast FilmCast Stretch FilmCollation ShrinkFood packagingForm Fill and Seal PackagingHeavy Duty BagsLamination FilmMultilayer Packaging FilmShrink FilmStand Up PouchesStretch FilmInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 2000 ppm
2000 ppm
Slip Level 500 ppm
500 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.3 MPa
1500 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ASTM D882
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 470 %
470 %
ASTM D882
Puncture Energy 3.62 J
2.67 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 90 g
90 g
ASTM D1922
Elmendorf Tear Strength TD 580 g
580 g
ASTM D1922
Dart Drop Test 210 g
0.463 lb
ASTM D1709A
Film Tensile Strength at Break, MD 60.0 MPa
8700 psi
ASTM D882
Film Tensile Strength at Break, TD 55.8 MPa
8100 psi
ASTM D882
1% Secant Modulus, MD 214 MPa
31000 psi
ASTM D882
1% Secant Modulus, TD 241 MPa
35000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
ASTM D1003
Gloss 56 %
56 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 12 lbf
ExxonMobil Method