Material Notes:
Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000 designation EJ, FK. Satisfactory compatibility with lubricating, fuel, and hydraulic oils, vegetable oils and animal fats, aliphatic hydrocarbon, alcohols, and water above or below 80°C.Applications include shaft seals, engine gaskets, radiators seals, transmission seals, valve lifter seals, vibration damping systems, valve stem seals, O-rings, hose, tubing, coated fabric, business machine rollers, and wire insulation/jacketing.Information provided by DuPont Dow Elastomers.This former DuPont Dow Elastomers Advanta® product line is not listed in the product lines of either Dow Chemical or DuPont Performance Elastomers.
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 90
60 - 90
Tensile Strength, Ultimate 12.0 - 15.0 MPa
1740 - 2180 psi
Elongation at Break 200 - 400 %
200 - 400 %
100% Modulus 0.00200 - 0.0120 GPa
0.290 - 1.74 ksi
Compression Set 25 - 30 %

@Temperature 165 °C
25 - 30 %

@Temperature 329 °F
70 hr at 165°C.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 175 °C
347 °F
Continuous service
Minimum Service Temperature, Air -12.0 °C
10.4 °F
Temperature retraction (TR-10)
Brittleness Temperature -20.0 °C
-4.00 °F
Brittle point
Glass Transition Temp, Tg -16.0 °C
3.20 °F
Inflection