Material Notes:
A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Viscosity 300 - 600 cP
300 - 600 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
ASTM D2240
Adhesive Bond Strength 19.3 MPa
2800 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear >= 50.0 µm/m-°C
>= 27.8 µin/in-°F
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 65.0 °C
149 °F
Optical Properties Metric English Comments
Refractive Index 1.52
1.52
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 65.0 °C
3.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 480 min
480 min