Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Riblene® MP 31 Low Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® MP 31 Low Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Riblene MP 31 is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 are characterized by a medium rigidity.Main Applications: Riblene MP 31 is suitable for injection molding and compound applications. Riblene MP 31 is recommended for caps, stoppers, closures and medium thickness articles.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.924 g/cc
0.924 g/cc
ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ISO 868/A
Tensile Strength, Yield 12.0 MPa
1740 psi
ISO 527
Flexural Modulus 0.200 GPa
29.0 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 112 °C
234 °F
Internal method
Vicat Softening Point 92.0 °C

@Load 1.00 kg
198 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -65.0 °C
<= -85.0 °F
ASTM D746