Ovation Polymers Nima™ NH OPP66GF25 FR 25% Glass Filled Polyamide 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ovation Polymers
Trade Name Nima™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nima™ NH OPP66GF25 FR 25% Glass Filled Polyamide 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Non-Hal red phosphorous based Flame Retardant CompoundAll properties after 48hrs conditioning at 23°C/50% RH
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.013 cm/cm

@Thickness 3.17 mm
0.0050 - 0.013 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.0050 - 0.016 cm/cm

@Thickness 3.17 mm
0.0050 - 0.016 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 103 MPa
14900 psi
50 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
50 mm/min; ASTM D638
Tensile Modulus 3.70 GPa
537 ksi
50 mm/min; ASTM D638
Flexural Strength 150 MPa
21800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.694 J/cm

@Temperature 23.0 °C
1.30 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 180 °C

@Thickness 3.20 mm
356 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0