Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CEN® Electronic Material BL Polyimide Film

Category Polymer , Thermoset , Polyimide, TS , Polyimide, Thermoset Film
Manufacturer CEN® Electronic Material Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CEN® Electronic Material BL Polyimide Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CEN®BL polyimide film is a printable film that has the same thermal and chemical properties as CEN®CN Polyimide Film, which offers excellent performance in temperatures from -269-400°C. CEN®BL is pigmented to provide contrast and eliminate the need for opaque coatings. Printing on BL can be accomplished with thermal transfer and laser printing.Applications: Labels for high temperature, cryogenic storage, harsh chemical environments, and printed circuit board identification.All information provided by CEN Electronic Material Co., LTD.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
Thickness 46.0 - 54.0 microns
1.81 - 2.13 mil
ASTM D374
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 145 MPa
21000 psi
ASTM D882
Film Tensile Strength at Yield, TD 135 MPa
19600 psi
ASTM D882
Elongation at Yield >= 45 %
>= 45 %
ASTM D882
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved