EMS-Grivory Grivory® L 25 W 20 Y PA12-I

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® L 25 W 20 Y PA12-I.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Grilamid L 25 W 20 Y black 9992 is a semiflexible plasticized, medium viscosity, extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 Y black 9992 is impact modified, heat and UV stabilized. The main features of Grilamid L 25 W 20 Y black 9992 are: High burst pressureExceptional impact strength also at low temperaturesComplies with the requirements of DIN 73378 class PA12 PHLYSemi-flexibleUV and heat stabilityGood chemical resistanceLow density, low weightEasy processing Application examples: Grilamid L 25 W 20 Y black 9992 is particularly suitable for the production of semiflexible tubes requiring good cold temperature impact strength with high burst pressure for use in automotive and industrial applications.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption 1.5 %
1.5 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
conditioned, 15s; ISO 868
Tensile Strength at Break 40.0 MPa
5800 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 30.0 MPa
4350 psi
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
>= 50 %
>= 50 %
dry; ISO 527-1/-2
Elongation at Yield 20 %
20 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.500 GPa
72.5 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Air intake sytems
Compressed air systems
Fuel systems
Hydraulic systems
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes Flexible
High viscosity
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)