Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide. Grivory GVX-7H black 9915 has an optimized flowability and is suitable for injection molding technical parts, exhibiting exceptional characteristics even after moisture absorption: high stiffness and strengthhigh dimensional stability, very low warpagegood chemical resistancevery good surface finish Grivory GVX-7H black 9915 is the economical alternative to die-cast alloys.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ISO 1183
Water Absorption 2.9 %
2.9 %
ISO 62
Moisture Absorption 1.00 %
1.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0020 cm/cm
0.0020 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 360 MPa
52200 psi
conditioned; ISO 2039-1
370 MPa
53700 psi
dry; ISO 2039-1
Tensile Strength at Break 260 MPa
37700 psi
conditioned; ISO 527-1/-2
290 MPa
42100 psi
dry; ISO 527-1/-2
Elongation at Break 1.5 %
1.5 %
dry; ISO 527-1/-2
1.5 %
1.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 27.5 GPa
3990 ksi
conditioned; ISO 527-1/-2
28.0 GPa
4060 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
dry; ISO 179/1eU
6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
dry; ISO 179/1eA
1.50 J/cm²
7.14 ft-lb/in²
conditioned; ISO 179/1eA
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 30.0 µm/m-°C
16.7 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
dry; IEC 60093
1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 33.0 kV/mm
838 kV/in
dry; IEC 60243-1
33.0 kV/mm
838 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Automotive electr. and electronics, lighting
Cooling and climate control
Exterior
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Sanitary, water and gas supply
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding
Partially aromatic Polyamide
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved