TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0N99030.0Coumarone-Indene Resin10.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.50All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
Mooney Viscosity 23

@Temperature 121 °C
23

@Temperature 250 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
Tensile Strength, Yield 33.8 MPa
4900 psi
Elongation at Yield 560 %
560 %
100% Modulus 0.00172 GPa
0.250 ksi
300% Modulus 0.00621 GPa
0.900 ksi
Tear Strength 37.8 kN/m
216 pli
Graves
Abrasion 55
55
NBS Index
Compression Set 20 %
20 %
Method B
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 142 °C
1.00 hour

@Temperature 287 °F