| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
| Melt Flow | 5.0 g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C |
5.0 g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 26.0 MPa <br>@Temperature 23.0 °C |
3770 psi <br>@Temperature 73.4 °F |
ISO 527 (1BA bar) |
| Tensile Stress | 2.00 MPa <br>@Strain 10.0 %,<br> Temperature 23.0 °C |
290 psi <br>@Strain 10.0 %,<br> Temperature 73.4 °F |
ISO 527 (1BA bar) |
| Elongation at Break | 650 % <br>@Temperature 23.0 °C |
650 % <br>@Temperature 73.4 °F |
ISO 527 (1BA bar) |
| Flexural Modulus | 0.0140 GPa <br>@Temperature 100 °C |
2.03 ksi <br>@Temperature 212 °F |
ISO 178 |
| 0.0280 GPa <br>@Temperature 23.0 °C |
4.06 ksi <br>@Temperature 73.4 °F |
ISO 178 | |
| 0.145 GPa <br>@Temperature -40.0 °C |
21.0 ksi <br>@Temperature -40.0 °F |
ISO 178 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 170 °C | 338 °F | 10°C/min; ISO 11357-1/-3 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 200 - 210 °C | 392 - 410 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | |
| Forms | Pellets | |
| Generic | TPC-ET | |
| Material Status | Preliminary Data | |
| Processing Method | Injection Molding | |
| Product Category | Food Contact Resins | |
| Region Available - Global | Yes | |
| RoHS Compliance | Contact Manufacturer | |
| Uses | Food Applications, Non-specific |