Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning HM-2510 CLEAR ASSEMBLY SEALANT

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning HM-2510 CLEAR ASSEMBLY SEALANT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc

@Temperature 25.0 °C
1.07 g/cc

@Temperature 77.0 °F
Volatiles <= 1.5 %
<= 1.5 %
Viscosity 105000 cP
105000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 47
47
Tensile Strength, Ultimate 2.69 MPa
390 psi
Elongation at Break 760 %
760 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Cure Time 2880 min

@Temperature 22.0 °C
48.0 hour

@Temperature 71.6 °F
Pot Life 1440 min
1440 min
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance clear
Users viewing this material also viewed the following: