| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.970 g/cc <br>@Temperature 25.0 °C |
0.970 g/cc <br>@Temperature 77.0 °F |
|
| Viscosity | 550 cP | 550 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 45 | 45 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | |
| Dielectric Constant | 2.87 <br>@Frequency 100 Hz |
2.87 <br>@Frequency 100 Hz |
|
| 2.87 <br>@Frequency 100000 Hz |
2.87 <br>@Frequency 100000 Hz |
||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | |
| Dissipation Factor | 0.00010 <br>@Frequency 100000 Hz |
0.00010 <br>@Frequency 100000 Hz |
|
| 0.0030 <br>@Frequency 100 Hz |
0.0030 <br>@Frequency 100 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 105 min <br>@Temperature 100 °C |
1.75 hour <br>@Temperature 212 °F |
|
| 180 min <br>@Temperature 80.0 °C |
3.00 hour <br>@Temperature 176 °F |
||
| 240 min <br>@Temperature 22.0 °C |
4.00 hour <br>@Temperature 71.6 °F |
||
| Shelf Life | 12.0 Month | 12.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | clear | |
| Flowable | yes | |
| Gel Hardness (Grams/Penetration) | 120 | |
| Hydrophobic | yes | |
| Self Leveling | yes | |
| Water Resistant | yes | |
| Working Time (min) | 30 |