| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnite® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Arnite® B604T PBT-I.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
| Water Absorption | 0.40 % | 0.40 % | Sim. To ISO 62 |
| Moisture Absorption | 0.150 % | 0.150 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO 527-1/-2 |
| Elongation at Break | 15 % | 15 % | ISO 527-1/-2 |
| Elongation at Yield | 3.2 % | 3.2 % | ISO 527-1/-2 |
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 95.0 µm/m-°C | 52.8 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 95.0 µm/m-°C | 52.8 µin/in-°F | ISO 11359-1/-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 125 °C | 257 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |