Cytec (Conap) RN-1000 / EA-87 Conapoxy® Resin / Conacure® Hardener

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Cytec
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec (Conap) RN-1000 / EA-87 Conapoxy® Resin / Conacure® Hardener.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive and related industries.Cytec (Conap) RN-1000 / EA-87 Conapoxy® Resin / Conacure® HardenerAn unfilled, low viscosity casting system recommended for potting and encapsulating resistors, connectors, solenoids, transformers, coils, and other electrical devices.Mix Ratio, Resin/Hardener (by weight): 100/37 Cure Type: Room Temperature
Physical Properties Metric English Comments
Viscosity 250 cP

@Temperature 25.0 °C
250 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 9.00e+15 ohm-cm
<= 9.00e+15 ohm-cm
Dielectric Constant 5.0

@Frequency 1000 Hz
5.0

@Frequency 1000 Hz
Dielectric Strength 13.8 kV/mm
350 kV/in
Dissipation Factor 0.040

@Frequency 1000 Hz
0.040

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 90.0 min

@Temperature 25.0 °C
90.0 min

@Temperature 77.0 °F
100 grams