DuPont Teijin Films Mylar® OL2 Polyester Film, 50 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® OL2 Polyester Film, 50 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and frozen foods. Mylar® OL2 is commercially available in nominal 50, 75 and 100 gauges. Mylar® OL2 is dual ovenable film which provides good, generally peelable seals to polar substrates such as amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, and polyvinylchloride (PVC). Mylar® OL2 does not seal to polyethylene, polypropylene, or polystyrene. DuPont Teijin Films offers another family of lidding films (RL types) for sealing to these substrates. Similar to Mylar® OL, heat seals with Mylar® OL2 are designed to be self venting and generally strippable from the above containers. Mylar® OL2 has a thicker seal layer than Mylar® OL and is recommended when the sealant thickness of Mylar® OL is not sufficient to make intimate contact with mating surface of the container. Mylar® OL2 produces higher seal strengths to most substrates than does Mylar® OL, and lower gauges tend to shred (film tear or break) more than Mylar® OL when peeled in cold environments. Shredding (film tear or break) can be minimized by using higher gauges.Corona Treatment (Mylar® OL2T): Selected gauges of Mylar® OL2 are available with corona treatment (on the side opposite the heat seal layer) to enhance printing and laminating. This film type is marketed by DuPont Teijin Films as Mylar® OL2T. The film is treated to an initial dyne level of 54. The dyne level of treated lidding films may decline with storage, and in-line corona treatment may be required during subsequent printing or laminating to increase the dyne level to a value adequate to get desired ink or laminate adhesion. Standard put-ups for Mylar® OL2T are the same as shown for Mylar® OL2. Anti-fog (Mylar® OLAF, OLAT): Selected gauges of Mylar® OL2 lidding films are available with anti-fogging capability to provide better clarity when stored and displayed in refrigerated conditions. This film type is marketed by DuPont Teijin Films as Mylar® OLAF. Mylar® OLAF is also available with corona treatment on the side opposite the heat seal layer. This film is marketed by DuPont Teijin Films as Mylar® OLAT.Approvals: FDA Food Contact Status - All gauges of Mylar® OL2 and OL2T comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Mylar® OL2 and OL2T can be used to contain foods during oven cooking or oven baking at temperatures above 250°F. (Note: This claim also applies to Mylar® OLAF and OLAT).Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Water Vapor Transmission 43.5 g/m²/day

@Temperature 38.0 °C
2.80 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 110 %
110 %
ASTM D882A
Film Elongation at Break, TD 80 %
80 %
ASTM D882A
Tensile Modulus 3.79 GPa
550 ksi
ASTM D882
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
Film Tensile Strength at Break, MD 172 MPa
25000 psi
ASTM D882A
Film Tensile Strength at Break, TD 241 MPa
35000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Descriptive Properties Value Comments
Gas Permeability (Base film) 9 cc/100 in2
O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal) 34600 in2/lb