Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
Tensile Strength, Ultimate 110 MPa
16000 psi
ASTM D638
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ASTM D638
Flexural Yield Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 17.0 GPa
2470 ksi
ASTM D790
Compressive Yield Strength 128 MPa
18600 psi
ASTM D695
Shear Strength 76.0 MPa
11000 psi
ASTM D732
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Specific Heat Capacity 0.770 J/g-°C
0.184 BTU/lb-°F
0.774 J/g-°C
0.185 BTU/lb-°F
Thermal Conductivity 0.560 W/m-K
3.89 BTU-in/hr-ft²-°F
Melting Point 285 °C
545 °F
Maximum Service Temperature, Air 230 °C
446 °F
UL temperature Index 220/240°C (430/460°F)
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Glass Transition Temp, Tg 88.0 °C
190 °F
Flammability, UL94 5VA
5VA
V-0/5VA UL-94 Rating
Oxygen Index 53 %
53 %
ASTM D2863
53 %
53 %
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+15 ohm-cm
5.00e+15 ohm-cm
ASTM D257
Surface Resistance 2.00e+8 ohm

@Temperature 90.0 °C
2.00e+8 ohm

@Temperature 194 °F
95% RH, 48 hrs
Dielectric Constant 5.8

@Frequency 1000 Hz
5.8

@Frequency 1000 Hz
ASTM D150
5.8

@Frequency 1e+6 Hz
5.8

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149
Dissipation Factor 0.029

@Frequency 1e+6 Hz
0.029

@Frequency 1e+6 Hz
ASTM D150
0.030

@Frequency 1000 Hz
0.030

@Frequency 1000 Hz
ASTM D150
Arc Resistance 116 sec
116 sec
ASTM D495
Comparative Tracking Index 160 V
160 V
UL 746A
Processing Properties Metric English Comments
Melt Temperature 304 - 343 °C
579 - 649 °F