Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic N66C2 Nylon 66, 20% Mineral Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Mineral Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Cheng Yu Plastic N66C2 Nylon 66, 20% Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.020 cm/cm
0.0020 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
ASTM D785
Tensile Strength, Yield 88.3 MPa
12800 psi
ASTM D638
Flexural Yield Strength 118 MPa
17100 psi
ASTM D790
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
ASTM D648
Flammability, UL94 HB
HB