Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® N120L (Dry) Nylon 6, 20% Glass Fiber Reinforced, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N120L (Dry) Nylon 6, 20% Glass Fiber Reinforced, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: LubricatedForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Filler Content 20 %
20 %
Water Absorption 1.4 %
1.4 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 134 MPa
19500 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
Unannealed; ASTM D648