Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 457 microns
18.0 mil
Side 1
457 microns
18.0 mil
Side 2
813 microns
32.0 mil
Prime Coated 3784 Fiberglass, Substrate
1600 - 1850 microns
63.0 - 73.0 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 55
45 - 55
Compound Property
Tensile Strength >= 6.55 MPa
>= 950 psi
Compound Property
Elongation at Break >= 700 %
>= 700 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Continuous
Electrical Properties Metric English Comments
Dielectric Strength <= 15.7 kV/mm
<= 400 kV/in
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.9 °C
60.0 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
Total Product Weight (oz/yd2) 64.5 - 78.5
Uncoated Fabric Break Strength 300 lb/in
Fill Direction, Substrate Property
350 lb/in
Warp Direction, Substrate Property
Users viewing this material also viewed the following: