Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carpenter Micro-Melt® M-42 Alloy (AISI M42)

Category Metal , Ferrous Metal , Tool Steel
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name Micro-Melt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter Micro-Melt® M-42 Alloy (AISI M42).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Micro-Melt® M-42 alloy is a powder metal super-high-speed steel possessing a hardness capability of Rockwell C 68/70. This alloy has been used for cutting tools in the toughest machining operations. The advantages of Micro-Melt premium high speed steels include ease of grinding, response to heat treatment, more uniform structure, greater wear resistance and improved toughness. In addition, Carpenter's unique hot rolling and rotary forging capabilities impart minimal distortion characteristics to these alloys.Applications: Twist drills, Turning tools, End mills, Milling cutters, Broaches, Router Bits, Form tools, Keyway cutters, Dovetail tools, Flycutters, Thread rolling dies, Tool bitsInformation provided by Carpenter Technology Corporation.Micro-Melt® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Specific Gravity 7.98 g/cc
7.98 g/cc
Mechanical Properties Metric English Comments
Hardness, Rockwell C 64 - 66
64 - 66
As quenched
65 - 67
65 - 67
Tempered at 1100°F
Modulus of Elasticity 206.8 GPa
29990 ksi
Izod Impact Unnotched 14.9 - 31.2 J
11.0 - 23.0 ft-lb
Component Elements Properties Metric English Comments
Carbon, C 1.1 %
1.1 %
Chromium, Cr 3.75 %
3.75 %
Cobalt, Co 8.25 %
8.25 %
Iron, Fe 74.69 %
74.69 %
As Balance
Molybdenum, Mo 9.5 %
9.5 %
Sulfur, S 0.060 %
0.060 %
Tungsten, W 1.5 %
1.5 %
Vanadium, V 1.15 %
1.15 %
Users viewing this material also viewed the following: