Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction

Category Metal , Nonferrous Metal , Cobalt Alloy , Nickel Alloy , Superalloy
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ductility and toughness, and excellent corrosion resistance. In addition, this alloy displays exceptional resistance to sulfidation, high temperature oxidation, and hydrogen embrittlement. The unique properties of MP35N alloy are developed through work hardening, phase transformation and aging. If the alloy is used in the fully work hardened condition, service temperatures up to 750°F (399°C) are suggested. MP35N alloy is normally produced by vacuum induction melting (VIM), followed vacuum arc remelting (VAR).Because of its unique combination of properties, MP35N alloy has been used in a wide variety of applications. MP35N alloy has been used in fasteners, springs, nonmagnetic electrical components and instrument parts in medical, seawater, oil and gas well, and chemical and food processing environments.*MP35N is a trademark of SPS Technologies, Inc. MP is a registered trademark of SPS Technologies, Inc.
Physical Properties Metric English Comments
Density 8.43 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1069 MPa
155000 psi
Tensile Strength, Yield 814 MPa
<br>@Strain 0.200 %
118000 psi
<br>@Strain 0.200 %
Elongation at Break 41 %
41 %
Reduction of Area 70 %
70 %
Modulus of Elasticity 234.8 GPa
34060 ksi
Shear Modulus 80.95 GPa
11740 ksi
Thermal Properties Metric English Comments
CTE, linear 12.8 µm/m-°C
<br>@Temperature 21.0 - 93.0 °C
7.11 µin/in-°F
<br>@Temperature 69.8 - 199 °F
14.8 µm/m-°C
<br>@Temperature 21.0 - 316 °C
8.22 µin/in-°F
<br>@Temperature 69.8 - 601 °F
15.7 µm/m-°C
<br>@Temperature 21.0 - 538 °C
8.72 µin/in-°F
<br>@Temperature 69.8 - 1000 °F
Thermal Conductivity 11.2 W/m-K
<br>@Temperature 23.0 °C
77.7 BTU-in/hr-ft²-°F
<br>@Temperature 73.4 °F
17.0 W/m-K
<br>@Temperature 316 °C
118 BTU-in/hr-ft²-°F
<br>@Temperature 601 °F
23.4 W/m-K
<br>@Temperature 649 °C
162 BTU-in/hr-ft²-°F
<br>@Temperature 1200 °F
Melting Point 1315 - 1440 °C
2399 - 2620 °F
Solidus 1315 °C
2399 °F
Liquidus 1440 °C
2620 °F
Component Elements Properties Metric English Comments
Boron, B 0.010 %
0.010 %
Carbon, C <= 0.025 %
<= 0.025 %
Chromium, Cr 19 - 21 %
19 - 21 %
Cobalt, Co 33 %
33 %
as remainder
Iron, Fe <= 1.0 %
<= 1.0 %
Manganese, Mn <= 0.15 %
<= 0.15 %
Molybdenum, Mo 9.0 - 10.5 %
9.0 - 10.5 %
Nickel, Ni 33 - 37 %
33 - 37 %
Phosphorous, P <= 0.015 %
<= 0.015 %
Silicon, Si <= 0.15 %
<= 0.15 %
Sulfur, S <= 0.010 %
<= 0.010 %
Titanium, Ti <= 1.0 %
<= 1.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001033 ohm-cm
<br>@Temperature 23.0 °C
0.0001033 ohm-cm
<br>@Temperature 73.4 °F
0.0001154 ohm-cm
<br>@Temperature 538 °C
0.0001154 ohm-cm
<br>@Temperature 1000 °F