Material Notes:
Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to welding and has very few contact applications. Electroplated coatings of gold on silver and other base metals are used in dry circuit application and to provide long shelf life reliability. Gold is alloyed with other metals to improve hardness, contact performance, and reduce cost.ELKONIUM® 76 is CMW's gold-copper alloy that is completely tarnish resistant at ordinary atmospheric temperatures. Compared to the other CMW gold ELKONIUM alloys, it has improved resistance to welding, and particularly cold welding. When used as a positive contact operating against an ELKONIUM 32 alloy negative contact in low voltage DC applications, the combination resists transfer and sticking at currents up to 4 amperes.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 17.3 g/cc
0.625 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 76
76
annealed
91
91
cold worked
Tensile Strength, Ultimate 400 MPa
58000 psi
annealed
703 MPa
102000 psi
cold worked
Elongation at Break 2.0 %
2.0 %
cold worked
25 %
25 %
annealed
Component Elements Properties Metric English Comments
Copper, Cu 10 %
10 %
Gold, Au 90 %
90 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000123 ohm-cm
0.0000123 ohm-cm
14 % IACS