Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name Perlast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resistance coupled with easy identification is required. Particularly suited for the Chemical Process and Analytical Science industries. Do not use any Perlast ® grade with molten alkali metals.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
71
71
°IRHD, +1 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 10.53 MPa
1527 psi
-35% change after 72 hours @ 250°C; ASTM D412
16.2 MPa
2350 psi
ASTM D412
Elongation at Break 154 %
154 %
ASTM D412
169.4 %
169.4 %
10% change after 72 hours @ 250°C; ASTM D412
100% Modulus 0.00959 GPa
1.39 ksi
-30% change after 72 hours @ 250°C; ASTM D412
0.0137 GPa
1.99 ksi
ASTM D412
Compression Set 35 %
35 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Flash Point >= 400 °C
>= 752 °F
Users viewing this material also viewed the following: