CMW® D505F Silver Nickel Contact Material

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer CMW Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® D505F Silver Nickel Contact Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
For electrical contacts.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.42 g/cc
0.3764 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F 32 - 84
32 - 84
32 (annealed) - 84 (worked)
Tensile Strength, Ultimate 165 MPa
23900 psi
Annealed
220 MPa
31900 psi
Worked
Thermal Properties Metric English Comments
Melting Point <= 1453 °C
<= 2647 °F
Liquidus 1453 °C
2647 °F
Component Elements Properties Metric English Comments
Nickel, Ni 5.0 %
5.0 %
Silver, Ag 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000181 ohm-cm
0.00000181 ohm-cm
(95% IACS)