Material Notes:
HYTAC-WF is an excellent high temperature epoxy syntactic material that provides improved clarity when forming APET and other clear polymers plus reduces sticking of difficult to process polymers such as HDPE or CPET. Dimensionally Stable:The low coefficient of thermal expansion means the plug maintains its shape over a wide temperature range.Smooth Surface: The glass sphere used in HYTAC-WF has a diameter more than 50% lower than those found in conventional syntactic materials, which translates to a smoother surface. Excellent Temperature Resistance: HYTAC-WF is specially formulated with an epoxy resin that maintains a high modulus at elevated temperatures. Lightweight: This increases the life of capital equipment due to reduced wear and tear on moving parts. Easily Machined: HYTAC-WF can be easily machined to any size or shape using conventional equipment. Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet the specific needs. Applications: HYTAC-WF utilizes microspheres with a diameter less than half the size of those used in conventional epoxy syntactic foams. This results in a surface that may be easily polished to a very smooth surface for improved part clarity. Recommended for use with APET, CPET, HDPE, OPS, PC, PETG, PMMA, PVC and RPETInformation Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.849 - 0.913 g/cc
0.0307 - 0.0330 lb/in³
Mechanical Properties Metric English Comments
Flexural Toughness 0.0324 MPa
4.70 psi
ASTM D790
Compressive Strength 124 MPa
18000 psi
Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C
18.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C
450 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Color White