Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic

Category Polymer , Thermoset , Epoxy
Manufacturer CMT Materials
Trade Name HYTAC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. The formulation has been designed to minimize chilling of the sheet and bring more material into the tool resulting in improved material distribution. FLX may be used in plug applications with a wide range of polymer sheet material and provides easy machining and polishing plus very good curability. As compared to standard thermoset epoxy syntactics, FLX has nearly 3X the flexural toughness and more than 4X the elongation to break. FLX has these outstanding attributes: Minimal to no scratching Good dimensional stability Excellent toughness and durability Good machinabilityTemperature resistanceLow thermal conductivity Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet the specific needs. Applications: HYTAC-FLX is a top choice for optical clarity with PET, provides excellent polymer yields as a result of better material distribution, lower starting gauge requirements and is more than double the flexural toughness of standard syntactic foams. Recommended for use with APET, CPET, HIPS, OPS, PETG, PLA, PP, PVC and RPET.Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.705 - 0.769 g/cc
0.0255 - 0.0278 lb/in³
Mechanical Properties Metric English Comments
Flexural Toughness 0.0524 MPa
7.60 psi
ASTM D790
Compressive Strength 92.05 MPa
13350 psi
Thermal Properties Metric English Comments
CTE, linear 41.4 µm/m-°C
23.0 µin/in-°F
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Descriptive Properties Value Comments
Color Pink