Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP FLEX D6520 T BLK Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resistanceGood UV resistanceLow densityWide service range from -20°C to 120°CProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0053 - 0.0059 cm/cm
0.0053 - 0.0059 in/in
ASTM D955
Melt Flow 10 - 15 g/10 min
10 - 15 g/10 min
ASTM D1238
Ash 25 - 30 %
25 - 30 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 16.5 MPa
>= 2400 psi
ASTM D638
Flexural Modulus >= 1.38 GPa
>= 200 ksi
ASTM D790
Izod Impact, Notched >= 0.534 J/cm

@Temperature -30.0 °C
>= 1.00 ft-lb/in

@Temperature -22.0 °F
ASTM D256
>= 1.60 J/cm

@Temperature 23.0 °C
>= 3.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256